A part that fills on one cycle and is short on another does not by itself prove hydraulic pressure instability. Start with the observed part and process sequence before changing pressure or temperature.
Record the Pattern
- Which cavities are affected, how often, and whether the issue starts after warmup, waiting or a material change.
- Material grade and lot, preparation, feeding and permitted regrind.
- Metered shot, cushion, recovery time, actual filling time and transfer behavior where available.
- Alarms, selected and actual traces, temperature readings and other simultaneous findings.
Separate the Investigation Areas
Review material delivery and preparation, plasticizing consistency, nozzle and flow-path condition, tooling and venting, process response and the relevant equipment records. These are investigation areas, not a diagnosis that every short shot is caused by a blocked nozzle.
Identify what any pressure reading represents and where it is measured. Compare equivalent cycles and machine states, rather than unrelated peak values or control percentages.
Keep Corrective Work within the Approved Procedure
Do not use paper, improvised shims or packing at a nozzle connection as a generic repair. Leaks, suspected blockage or connection faults require the applicable stop, isolation and service procedures. Do not clear a suspected obstruction by simply increasing pressure or temperature.
Filling Questions
Should Every Intermittent Short Shot Be Corrected by More Pressure?
No. First establish the material, shot, filling and equipment evidence; a pressure increase can conceal another issue or introduce defects.
Can an Incomplete Part Alone Identify a Failed Pump?
No. Keep the finding separate from the cause and provide the relevant records for assessment.
Use pressure definitions and the service evidence checklist.